Local lattice parameter measurements in a creep-deformed nickel-base superalloy by convergent beam electron diffraction

Research output: Contribution to journalArticleResearchpeer review

Authors

External Research Organisations

  • Friedrich-Alexander-Universität Erlangen-Nürnberg (FAU Erlangen-Nürnberg)
View graph of relations

Details

Original languageEnglish
Pages (from-to)1167-1172
Number of pages6
JournalScripta Metallurgica et Materiala
Volume27
Issue number9
Publication statusPublished - 1 Nov 1992
Externally publishedYes

ASJC Scopus subject areas

Cite this

Local lattice parameter measurements in a creep-deformed nickel-base superalloy by convergent beam electron diffraction. / Keller, R. R.; Maier, H. J.; Renner, H. et al.
In: Scripta Metallurgica et Materiala, Vol. 27, No. 9, 01.11.1992, p. 1167-1172.

Research output: Contribution to journalArticleResearchpeer review

Download
@article{bb1900edd86a4ea2805e7ea9d8ea9c4b,
title = "Local lattice parameter measurements in a creep-deformed nickel-base superalloy by convergent beam electron diffraction",
author = "Keller, {R. R.} and Maier, {H. J.} and H. Renner and H. Mughrabi",
year = "1992",
month = nov,
day = "1",
doi = "10.1016/0956-716X(92)90593-4",
language = "English",
volume = "27",
pages = "1167--1172",
journal = "Scripta Metallurgica et Materiala",
issn = "0956-716X",
publisher = "Acta Materialia Inc",
number = "9",

}

Download

TY - JOUR

T1 - Local lattice parameter measurements in a creep-deformed nickel-base superalloy by convergent beam electron diffraction

AU - Keller, R. R.

AU - Maier, H. J.

AU - Renner, H.

AU - Mughrabi, H.

PY - 1992/11/1

Y1 - 1992/11/1

UR - http://www.scopus.com/inward/record.url?scp=0026943991&partnerID=8YFLogxK

U2 - 10.1016/0956-716X(92)90593-4

DO - 10.1016/0956-716X(92)90593-4

M3 - Article

AN - SCOPUS:0026943991

VL - 27

SP - 1167

EP - 1172

JO - Scripta Metallurgica et Materiala

JF - Scripta Metallurgica et Materiala

SN - 0956-716X

IS - 9

ER -